Name

thermal shock resistant clay brick

Brand

AKN-115

Al2O3Content,%

≥ 45

Fe2O3Content,%

≤2.0

Percent porosity,%

≤ 22

Bulk density, kg/cm³

≥ 2.15

Normal temperature compressive strength, MPa

≥ 40

Load softening start temperature 0.2Mpa ,T0.6,℃

≥ 1410

Rate of change of heating permanent line,%

1400 ℃ × 2h
-0.3~ 0.1

Thermal shock resistance, 1100 ℃ water cooling, times

≥ 20